1} SILICA+OXIDISED LANTHANUM+BORIC ACID AT TEMP 1200-1400 C.
2} DISSOLVED AND ADVANCED MOULDING IS DONE.
3} PURE SILICA Sio2 AT VISCOSITY 200P, M.P =200 C CONVERTED TO SODA LIME.
4} GRINDING AND FINE POLISHING IS DONE.
5} ANTI REFLECTIVE COATING IS DONE WITH FLUORINATED MAGNESIUM.
6} END MATERIAL IS OBTANIED AS MAGNIFYING GLASS.